INCONEL ® alloy 625

High strength and toughness from cryogenic temperatures to 1800 degrees F (980 degrees C), good oxidation resistance, exceptional fatigue strength, and good corrosion resistance.

Is Inconel 625 heat treatable?

Depending on customer requirements, alloy 625 may also be supplied solution heat-treated at temperatures at or above 2000°F (1093°C), or mill annealed at temperatures below 1925°F (1052°C).

What is the melting point of Inconel 625?

1290-1350°C
Properties of Alloy 625

DENSITY 8.44 g/cm³ | 0.305 lb/cu in
MELTING POINT 1290-1350°C | 2350-2460 °F

Is Inconel 625 NACE compliant?

Sour service material manufactured with Inconel 625 (UNS N06625) has to comply with ANSI/NACE MR0175/ISO 15156. NACE MR0175 provides the metallurgical requirements for Inconel 625. Metallurgical condition and hardness are two of those requirements discussed in this article.

Is Alloy 625 the same as Inconel?

Alloy 625 has excellent fatigue strength and stress – corrosion cracking resistance to chloride ions. INCONEL® 625 LCF is a variant of INCONEL® 625. LCF stands for Low Cycle Fatigue. This means that the alloy has improved cycle fatigue properties and better thermal fatigue resistance.

What is the difference between Inconel 625 and 718?

Overview. Both Inconel 625 and Inconel 718 are superalloys with excellent comprehensive properties. The main difference between them is that the performance of Inconel 625 is more towards corrosion resistance, while the performance of Inconel 718 is more towards high strength.

What is the Rockwell hardness of Inconel 625?

Mechanical Properties

Condition Form Hardness, Rockwell
Annealed at 1925°F (1052°C), rapid cooled Sheet 0.014-0.063″ thick B94
Annealed at 1925°F (1052°C), rapid cooled Sheet,* 0.0.78-0.155″ thick B97
Annealed at 1925°F (1052°C), rapid cooled Plate,*** 1/4″ 1/2″ 3/4″ 1.00″ 1-1/2″ 1-3/4″ B94 B98 B98 B97 B97 C20

What is the difference between Inconel 625 and 825?

The major difference between Inconel 625 and 825 is the nickel content; Inconel 625 contains about 58% of nickel while Inconel 825 contains about 36-48% of nickel. Moreover, they have different melting points as well. The melting point of Inconel 625 is 1350◦C, but it is 1400◦C for Inconel 825.

What is the hardness of Inconel 625?

What is the difference between Inconel 625 and Alloy 625?

What is Inconel 625 used for?

Typical marine applications of INCONEL 625 include steam liner bellows, sheathing for undersea communication cables, and various submarine components such as auxiliary propulsion motors and quick-disconnect fittings.

Can Inconel 625 be hardened?

The hardness of the nickel based superalloy Inconel 625, aged at 625, 700, and 760°C for different intervals of time ranging from 1 to 335 h, has been measured. Peak hardening is found to occur much earlier at 760°C than at 700°C.